Serial No. | Items being Tested | Standard Index | Test Value | |
1 | Tensile Strength of Cementation (with cement mortar): Mpa | Original Strength | ≥0.60 | 0.71 |
Waterproof | ≥0.40 | 0.52 | ||
2 | Tensile Strength of Cementation (with Polystyrene board): Mpa | Original Strength | ≥0.10 Destruction of Polystyrene Board | 0.12 Destruction of Polystyrene Board |
Waterproof | ≥0.10 Destruction of Polystyrene Board | 0.10 Destruction of Polystyrene Board | ||
3 | Operation Time Available: Hour | 1.2~4.0 | 2.0 |
Serial No. | Items being Tested | Standard Index | Test Value | |
1 | Tensile Strength of Cementation (with Polystyrene board): Mpa | Original Strength | ≥0.10 Destruction of Polystyrene Board | 0.11 Destruction of Polystyrene Board |
Waterproof | ≥0.10 Destruction of Polystyrene Board | 0.10 Destruction of Polystyrene Board | ||
Freeze-Thaw Resistance | ≥0.10 Destruction of Polystyrene Board | 0.10 Destruction of Polystyrene Board | ||
2 | Flexibility (compressive strength/flexural strength) | ≤3.0 | 2.7 | |
3 | Operation Time Available: Hour | 1.5~4.0 | 2.0 |